From 6df3f120c729f7b0d0bf8f49ab922c42d69d8404 Mon Sep 17 00:00:00 2001 From: Ferran Brosa Planella Date: Tue, 26 May 2020 18:38:50 +0200 Subject: [PATCH] #718 added parameters for arbitrary lumped model, assuming pouch --- .../input/parameters/lithium-ion/cells/Kim2011/parameters.csv | 2 ++ .../lithium-ion/cells/kokam_Ecker2015/parameters.csv | 2 ++ .../experiments/1C_charge_from_empty_Mohtat2020/parameters.csv | 1 + .../1C_discharge_from_full_Ecker2015/parameters.csv | 3 ++- .../experiments/1C_discharge_from_full_Kim2011/parameters.csv | 3 ++- 5 files changed, 9 insertions(+), 2 deletions(-) diff --git a/pybamm/input/parameters/lithium-ion/cells/Kim2011/parameters.csv b/pybamm/input/parameters/lithium-ion/cells/Kim2011/parameters.csv index 343f4559d1..c2af2dc9b1 100644 --- a/pybamm/input/parameters/lithium-ion/cells/Kim2011/parameters.csv +++ b/pybamm/input/parameters/lithium-ion/cells/Kim2011/parameters.csv @@ -15,6 +15,8 @@ Negative tab centre z-coordinate [m],0.2, At top, Positive tab width [m],0.044,, Positive tab centre y-coordinate [m],0.137,, Positive tab centre z-coordinate [m],0.2,At top, +Cell cooling surface area [m2],2.80E-2,,pouch +Cell volume [m3],4.62E-6,,pouch ,,, # Current collector properties ,,, Negative current collector conductivity [S.m-1],59.6E6,, diff --git a/pybamm/input/parameters/lithium-ion/cells/kokam_Ecker2015/parameters.csv b/pybamm/input/parameters/lithium-ion/cells/kokam_Ecker2015/parameters.csv index 4be97ac3af..86dcacc298 100644 --- a/pybamm/input/parameters/lithium-ion/cells/kokam_Ecker2015/parameters.csv +++ b/pybamm/input/parameters/lithium-ion/cells/kokam_Ecker2015/parameters.csv @@ -9,6 +9,8 @@ Positive electrode thickness [m],5.4E-05,, Positive current collector thickness [m],2.5E-05,, Electrode height [m],1.01E-01,, Electrode width [m],8.50E-02,, +Cell cooling surface area [m2],8.59E-3,,pouch (single layer) +Cell volume [m3],1.61E-6,,pouch (single layer) ,,, # Electrical,,, Cell capacity [A.h], 0.15625, 7.5/48 (parameter set for a single layer cell), diff --git a/pybamm/input/parameters/lithium-ion/experiments/1C_charge_from_empty_Mohtat2020/parameters.csv b/pybamm/input/parameters/lithium-ion/experiments/1C_charge_from_empty_Mohtat2020/parameters.csv index 57fcd59173..d1c0a2367c 100644 --- a/pybamm/input/parameters/lithium-ion/experiments/1C_charge_from_empty_Mohtat2020/parameters.csv +++ b/pybamm/input/parameters/lithium-ion/experiments/1C_charge_from_empty_Mohtat2020/parameters.csv @@ -8,6 +8,7 @@ Positive current collector surface heat transfer coefficient [W.m-2.K-1],0,, Negative tab heat transfer coefficient [W.m-2.K-1],0,, Positive tab heat transfer coefficient [W.m-2.K-1],0,, Edge heat transfer coefficient [W.m-2.K-1],5,Peyman MPM, +Total heat transfer coefficient [W.m-2.K-1],5,Peyman MPM, Ambient temperature [K], 298.15,, ,,, # Electrical diff --git a/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Ecker2015/parameters.csv b/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Ecker2015/parameters.csv index 0397997a1b..aca4beec45 100644 --- a/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Ecker2015/parameters.csv +++ b/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Ecker2015/parameters.csv @@ -8,7 +8,8 @@ Positive current collector surface heat transfer coefficient [W.m-2.K-1],0,Paper Negative tab heat transfer coefficient [W.m-2.K-1],10,Paper does not consider thermal effects, Positive tab heat transfer coefficient [W.m-2.K-1],10,Paper does not consider thermal effects, Edge heat transfer coefficient [W.m-2.K-1],0.3,Paper does not consider thermal effects, -Ambient temperature [K], 298.15,, +Total heat transfer coefficient [W.m-2.K-1],10,Paper does not consider thermal effects, +Ambient temperature [K],298.15,, ,,, # Electrical diff --git a/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Kim2011/parameters.csv b/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Kim2011/parameters.csv index 4d475c47e8..41be8dc122 100644 --- a/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Kim2011/parameters.csv +++ b/pybamm/input/parameters/lithium-ion/experiments/1C_discharge_from_full_Kim2011/parameters.csv @@ -8,7 +8,8 @@ Positive current collector surface heat transfer coefficient [W.m-2.K-1],0,, Negative tab heat transfer coefficient [W.m-2.K-1],25,, Positive tab heat transfer coefficient [W.m-2.K-1],25,, Edge heat transfer coefficient [W.m-2.K-1],0.3,, -Ambient temperature [K], 298.15,, +Total heat transfer coefficient [W.m-2.K-1],25,, +Ambient temperature [K],298.15,, ,,, # Electrical